Message ID: 77     Entry time: Mon Apr 24 17:38:45 2023
Author: Aiden 
Type: Summary 
Category: General 
Subject: Clean and Bake Batch 12 
Today I Bagged and tagged the o-rings from batch 11 and placed them inside the clean room. I also cleaned batch 12 parts in liquinox for 10 minutes and them placed them into the oven where they will undergo the following steps; 1. Ramp to 100 degC in 15 min. 2. Dwell at 100 degC for 30 min. 3. Ramp to 200 deg C in 30 min. 4. Dwell at 200 deg C for 48 hours. 5. Off